Hydration of Early-Age Concrete – Sequential Tunnel Casting


Disclaimer

The information contained herein has been prepared only for the purpose of demonstration. It should not be used for any

engineering design work and nothing should be inferred from its results or conclusion.


Introduction

This document provides a demonstration of the functionality of Strand7 and the key steps required to model and

solve concrete casting problems in the Strand7 finite element analysis system. This demonstration addresses

factors including concrete hydration, creep and shrinkage, sequential (staged) casting, as well as the

development of concrete stiffness with time. The Strand7 results are qualitatively compared to results obtained

from similar analyses performed by Hatel and Thorborg [1]. The results used for the comparison include

temperature and crack index profiles.


b45323f8d7618933de25396e014330f7_1612160694_41.gif
 

첨부파일

댓글목록

등록된 댓글이 없습니다.


그누보드5
  • 서울시 도봉구 도봉로106길 22, 201-508 (북한산현대홈시티) TEL : 02-529-0841 FAX : 02-529-0846
  • Copyright © CNG SOFTEK CO., LTD. All rights reserved.